Find suppliers for this alloyC93200
Chemical Composition
Element
Cu(1,2)PbSnZnFeP(3)Ni(4)AlSSbSi
(1) Cu + Sum of Named Elements 99.0% min. (2) In determining Cu min., Cu may be calculated as Cu + Ni. (3) For continuous castings P shall be 1.5% max. (4) Ni value includes Co.
Min (%)81.06.06.31.0
Max (%)85.08.07.54.00.200.151.00.0050.080.350.005
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
Brinell Hardness, 500 kg load
Izod
(ft-lbs)
Compressive Strength .1 in. set/in.
(ksi)
Fatigue Strength**
(ksi)
Proportional Limit
(ksi)
As Centrifugal CastAs Centrifugal CastM0230   Min for Standard
14   Min for Standard
15   Min for Standard
As Continuous CastAs Continuous CastM0735   Min for Standard
35   Min for Standard
20   Min for Standard
20   Min for Standard
10   Min for Standard
10   Min for Standard
As Sand CastAs Sand CastM0130   Min for Standard
30   Min for Standard
35   Typ
14   Min for Standard
14   Min for Standard
18   Typ
15   Min for Standard
15   Min for Standard
20   Typ
65   Typ
6   Typ
46   Typ
16   Typ
8.5   Typ
* Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106.
Physical Properties
Melting Point - Liquidus°F1790
Melting Point - Solidus°F1570
Densitylb/cu in. at 68°F0.322
Specific Gravity8.91
Electrical Conductivity% IACS at 68°F12
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F33.6
Coefficient of Thermal Expansion 68-21210⁻⁶ per °F (68 – 212°F)10
Specific Heat CapacityBtu/ lb /°F at 68°F0.09
Modulus of Elasticity in Tensionksi14500
Casting Characteristics
Casting Attribute Level
Casting YieldHigh
DrossingLow
Effect of Section SizeMedium
FluidityMedium
GassingMedium
Patternmakers Shrinkageinches per inch7/32
Shrinkage in SolidificationLow
Fabrication Properties
Technique Suitability Footnote
SolderingExcellent
BrazingGoodSince brazing is performed in the hot short temperature range, strain must be avoided during brazing and cooling.
Oxyacetylene WeldingNot Recommended
Gas Shielded Arc WeldingNot Recommended
Coated Metal Arc WeldingNot Recommended
Machinability Rating70
Common Fabrication Processes
  • Casting
    
Thermal Properties
Treatment Value* Time**
* Temperature is measured in Fahrenheit. ** Time is measured in minutes.
Stress Relief500
Solution Treatment0
Typical uses
Product Category Product Reason Category Reason
AutomotiveAutomotive FittingsCorrosion ResistanceCorrosion Resistance
Automotive FittingsCorrosion ResistanceCorrosion Resistance to Numerous Environments
Automotive FittingsMachining PropertiesMachinability, Good
Automotive FittingsMechanical PropertiesRelatively Low Strength
FastenersWashersCorrosion ResistanceCorrosion Resistance
WashersCorrosion ResistanceCorrosion Resistance to Numerous Environments
WashersMachining PropertiesMachinability, Good
WashersMechanical PropertiesRelatively Low Strength
IndustrialBearingsCorrosion ResistanceCorrosion Resistance
BearingsCorrosion ResistanceCorrosion Resistance to Numerous Environments
BearingsFriction & Wear PropertiesAnti-Seizing Properties
BearingsFriction & Wear PropertiesLow Coefficient of Friction
BearingsFriction & Wear PropertiesWear Resistance
BearingsMachining PropertiesMachinability, Good
BearingsMechanical PropertiesRelatively Low Strength
Bearings for CranesCorrosion ResistanceCorrosion Resistance
Bearings for CranesCorrosion ResistanceCorrosion Resistance to Numerous Environments
Bearings for CranesFriction & Wear PropertiesAnti-Seizing Properties
Bearings for CranesFriction & Wear PropertiesLow Coefficient of Friction
Bearings for CranesFriction & Wear PropertiesWear Resistance
Bearings for CranesMachining PropertiesMachinability, Good
Bearings for CranesMechanical PropertiesRelatively Low Strength
BushingsCorrosion ResistanceCorrosion Resistance
BushingsCorrosion ResistanceCorrosion Resistance to Numerous Environments
BushingsFriction & Wear PropertiesLow Coefficient of Friction
BushingsFriction & Wear PropertiesWear Resistance
BushingsMachining PropertiesMachinability, Good
BushingsMechanical PropertiesRelatively Low Strength
Diesel Engine Wrist Pin BushingsCorrosion ResistanceCorrosion Resistance
Diesel Engine Wrist Pin BushingsCorrosion ResistanceCorrosion Resistance to Many Industrial Chemicals
Diesel Engine Wrist Pin BushingsFriction & Wear PropertiesAnti-Seizing Properties
Diesel Engine Wrist Pin BushingsFriction & Wear PropertiesLow Coefficient of Friction
Diesel Engine Wrist Pin BushingsFriction & Wear PropertiesWear Resistance
Diesel Engine Wrist Pin BushingsMachining PropertiesMachinability, Good
Diesel Engine Wrist Pin BushingsMechanical PropertiesRelatively Low Strength
FittingsCorrosion ResistanceCorrosion Resistance
FittingsCorrosion ResistanceCorrosion Resistance to Numerous Environments
FittingsMachining PropertiesMachinability, Good
FittingsMechanical PropertiesRelatively Low Strength
Forging Press Toggle Lever BearingsCorrosion ResistanceCorrosion Resistance
Forging Press Toggle Lever BearingsCorrosion ResistanceCorrosion Resistance to Numerous Environments
Forging Press Toggle Lever BearingsFriction & Wear PropertiesAnti-Seizing Properties
Forging Press Toggle Lever BearingsFriction & Wear PropertiesLow Coefficient of Friction
Forging Press Toggle Lever BearingsFriction & Wear PropertiesWear Resistance
Forging Press Toggle Lever BearingsMachining PropertiesMachinability, Good
Forging Press Toggle Lever BearingsMechanical PropertiesRelatively Low Strength
Fuel Pump BushingsCorrosion ResistanceCorrosion Resistance
Fuel Pump BushingsCorrosion ResistanceCorrosion Resistance to Numerous Environments
Fuel Pump BushingsFriction & Wear PropertiesAnti-Seizing Properties
Fuel Pump BushingsFriction & Wear PropertiesLow Coefficient of Friction
Fuel Pump BushingsFriction & Wear PropertiesWear Resistance
Fuel Pump BushingsMachining PropertiesMachinability, Good
Fuel Pump BushingsMechanical PropertiesRelatively Low Strength
General Purpose BushingsCorrosion ResistanceCorrosion Resistance
General Purpose BushingsCorrosion ResistanceCorrosion Resistance to Numerous Environments
General Purpose BushingsFriction & Wear PropertiesAnti-Seizing Properties
General Purpose BushingsFriction & Wear PropertiesLow Coefficient of Friction
General Purpose BushingsFriction & Wear PropertiesWear Resistance
General Purpose BushingsMachining PropertiesMachinability, Good
General Purpose BushingsMechanical PropertiesRelatively Low Strength
Hydraulic Press Main LiningCorrosion ResistanceCorrosion Resistance
Hydraulic Press Main LiningCorrosion ResistanceCorrosion Resistance to Many Industrial Chemicals
Hydraulic Press Main LiningFriction & Wear PropertiesAnti-Seizing Properties
Hydraulic Press Main LiningFriction & Wear PropertiesWear Resistance
Hydraulic Press Main LiningMachining PropertiesMachinability, Good
Hydraulic Press Main LiningMechanical PropertiesRelatively Low Strength
Hydraulic Press Stuffing BoxCorrosion ResistanceCorrosion Resistance
Hydraulic Press Stuffing BoxCorrosion ResistanceCorrosion Resistance to Numerous Environments
Hydraulic Press Stuffing BoxMachining PropertiesMachinability, Good
Hydraulic Press Stuffing BoxMechanical PropertiesRelatively Low Strength
Hydraulic Press Stuffing BoxPressure TightPressure Tight
Insert BearingsCorrosion ResistanceCorrosion Resistance
Insert BearingsCorrosion ResistanceCorrosion Resistance to Numerous Environments
Insert BearingsFriction & Wear PropertiesLow Coefficient of Friction
Insert BearingsFriction & Wear PropertiesWear Resistance
Insert BearingsMachining PropertiesMachinability, Good
Insert BearingsMechanical PropertiesRelatively Low Strength
Linkage Bushings for PressesCorrosion ResistanceCorrosion Resistance
Linkage Bushings for PressesCorrosion ResistanceCorrosion Resistance to Numerous Environments
Linkage Bushings for PressesFriction & Wear PropertiesAnti-Seizing Properties
Linkage Bushings for PressesFriction & Wear PropertiesLow Coefficient of Friction
Linkage Bushings for PressesFriction & Wear PropertiesWear Resistance
Linkage Bushings for PressesMachining PropertiesMachinability, Good
Linkage Bushings for PressesMechanical PropertiesRelatively Low Strength
Machine PartsConductivity (Thermal)Thermal Conductivity
Machine PartsCorrosion ResistanceCorrosion Resistance
Machine PartsCorrosion ResistanceCorrosion Resistance to Numerous Environments
Machine PartsFriction & Wear PropertiesAnti-Seizing Properties
Machine PartsFriction & Wear PropertiesWear Resistance
Machine PartsMachining PropertiesMachinability, Good
Machine PartsMechanical PropertiesRelatively Low Strength
Machine Tool BearingsCorrosion ResistanceCorrosion Resistance
Machine Tool BearingsCorrosion ResistanceCorrosion Resistance to Numerous Environments
Machine Tool BearingsFriction & Wear PropertiesAnti-Seizing Properties
Machine Tool BearingsFriction & Wear PropertiesLow Coefficient of Friction
Machine Tool BearingsFriction & Wear PropertiesWear Resistance
Machine Tool BearingsMachining PropertiesMachinability, Good
Machine Tool BearingsMechanical PropertiesRelatively Low Strength
Main Spindle BearingsCorrosion ResistanceCorrosion Resistance
Main Spindle BearingsCorrosion ResistanceCorrosion Resistance to Numerous Environments
Main Spindle BearingsFriction & Wear PropertiesAnti-Seizing Properties
Main Spindle BearingsFriction & Wear PropertiesLow Coefficient of Friction
Main Spindle BearingsFriction & Wear PropertiesWear Resistance
Main Spindle BearingsMachining PropertiesMachinability, Good
Main Spindle BearingsMechanical PropertiesRelatively Low Strength
Pump FixturesCorrosion ResistanceCorrosion Resistance
Pump FixturesCorrosion ResistanceCorrosion Resistance to Numerous Environments
Pump FixturesMachining PropertiesMachinability, Good
Pump FixturesMechanical PropertiesRelatively Low Strength
Pump ImpellersCorrosion ResistanceCorrosion Resistance
Pump ImpellersCorrosion ResistanceCorrosion Resistance to Brackish Water
Pump ImpellersCorrosion ResistanceCorrosion Resistance to Many Industrial Chemicals
Pump ImpellersCorrosion ResistanceCorrosion Resistance to Numerous Environments
Pump ImpellersCorrosion ResistanceCorrosion Resistance to Petroleum Products
Pump ImpellersFriction & Wear PropertiesWear Resistance
Pump ImpellersMachining PropertiesMachinability, Good
Pump ImpellersMechanical PropertiesRelatively Low Strength
PumpsCorrosion ResistanceCorrosion Resistance
PumpsCorrosion ResistanceCorrosion Resistance to Brackish Water
PumpsCorrosion ResistanceCorrosion Resistance to Many Industrial Chemicals
PumpsCorrosion ResistanceCorrosion Resistance to Numerous Environments
PumpsFriction & Wear PropertiesWear Resistance
PumpsMachining PropertiesMachinability, Good
PumpsMechanical PropertiesRelatively Low Strength
PumpsPressure TightPressure Tight
Roll Neck BearingsCorrosion ResistanceCorrosion Resistance
Roll Neck BearingsCorrosion ResistanceCorrosion Resistance to Numerous Environments
Roll Neck BearingsFriction & Wear PropertiesLow Coefficient of Friction
Roll Neck BearingsFriction & Wear PropertiesWear Resistance
Roll Neck BearingsMachining PropertiesMachinability, Good
Roll Neck BearingsMechanical PropertiesRelatively Low Strength
Rolling Mill BearingsCorrosion ResistanceCorrosion Resistance
Rolling Mill BearingsCorrosion ResistanceCorrosion Resistance to Numerous Environments
Rolling Mill BearingsFriction & Wear PropertiesLow Coefficient of Friction
Rolling Mill BearingsFriction & Wear PropertiesWear Resistance
Rolling Mill BearingsMachining PropertiesMachinability, Good
Rolling Mill BearingsMechanical PropertiesRelatively Low Strength
Thrust WashersCorrosion ResistanceCorrosion Resistance
Thrust WashersCorrosion ResistanceCorrosion Resistance to Numerous Environments
Thrust WashersFriction & Wear PropertiesWear Resistance
Thrust WashersMachining PropertiesMachinability, Good
Thrust WashersMechanical PropertiesRelatively Low Strength
Trunion BearingsCorrosion ResistanceCorrosion Resistance
Trunion BearingsCorrosion ResistanceCorrosion Resistance to Numerous Environments
Trunion BearingsFriction & Wear PropertiesLow Coefficient of Friction
Trunion BearingsFriction & Wear PropertiesWear Resistance
Trunion BearingsMachining PropertiesMachinability, Good
Trunion BearingsMechanical PropertiesRelatively Low Strength
Water Pump BushingsCorrosion ResistanceCorrosion Resistance
Water Pump BushingsCorrosion ResistanceCorrosion Resistance to Brackish Water
Water Pump BushingsCorrosion ResistanceCorrosion Resistance to Many Industrial Chemicals
Water Pump BushingsFriction & Wear PropertiesAnti-Seizing Properties
Water Pump BushingsFriction & Wear PropertiesLow Coefficient of Friction
Water Pump BushingsFriction & Wear PropertiesWear Resistance
Water Pump BushingsMachining PropertiesMachinability, Good
Water Pump BushingsMechanical PropertiesRelatively Low Strength
Applicable Specifications
Form Sub-Form System Standard Description
As Centrifugal CastCastingsASTMB271/B271MCOPPER BASE ALLOY CENTRIFUGAL CASTINGS
CastingsSAEJ461WROUGHT AND CAST COPPER ALLOYS
CastingsSAEJ462CAST COPPER ALLOYS
As Continuous CastCastingsASTMB505/B505MCOPPER BASE ALLOY CONTINUOUS CASTINGS
CastingsSAEJ461WROUGHT AND CAST COPPER ALLOYS
CastingsSAEJ462CAST COPPER ALLOYS
As Permanent Mold CastCastingsSAEJ461WROUGHT AND CAST COPPER ALLOYS
CastingsSAEJ462CAST COPPER ALLOYS
As Sand CastCastingsASTMB584COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS
ASTMB66BRONZE CASTINGS IN THE ROUGH FOR LOCOMOTIVE WEARING PARTS
CastingsASTMB763/B763MCOPPER ALLOY SAND CASTINGS FOR VALVE APPLICATIONS
CastingsSAEJ461WROUGHT AND CAST COPPER ALLOYS
CastingsSAEJ462CAST COPPER ALLOYS
Ingot
ASTMB30COPPER BASE ALLOYS IN INGOT FORM
Corrosion Properties

No information available.