Find suppliers for this alloyC93600
Chemical Composition
Element
Cu(1)PbSnZnFeP(2)Ni(3)AlSSbSi
(1) Cu + Sum of Named Elements 99.3% min. (2) For continuous castings P shall be 1.5% max. (3) Ni value includes Co.
Min (%)79.011.06.0
Max (%)83.013.08.01.00.200.151.00.0050.080.550.005
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
Brinell Hardness, 500 kg load
As Centrifugal CastAs Centrifugal CastM0232   Min for Standard
35   Typ
16   Min for Standard
21   Typ
10   Min for Standard
15   Typ
65   Typ
As Continuous CastAs Continuous CastM0733   Min for Standard
35   Typ
20   Min for Standard
21   Typ
10   Min for Standard
15   Typ
65   Typ
As Permanent Mold CastAs Permanent Mold CastM0535   Typ
21   Typ
15   Typ
65   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1720
Melting Point - Solidus°F1550
Densitylb/cu in. at 68°F0.325
Specific Gravity9
Electrical Conductivity% IACS at 68°F11
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F28.5
Coefficient of Thermal Expansion 68-39210⁻⁶ per °F (68 – 392°F)10.3
Specific Heat CapacityBtu/ lb /°F at 68°F0.09
Modulus of Elasticity in Tensionksi14000
Casting Characteristics
Casting Attribute Level
Casting YieldHigh
DrossingLow
Effect of Section SizeLow
FluidityHigh
GassingMedium
Patternmakers Shrinkageinches per inch2/16
Shrinkage in SolidificationLow
Fabrication Properties
Technique Suitability
SolderingGood
BrazingGood
Oxyacetylene WeldingNot Recommended
Gas Shielded Arc WeldingNot Recommended
Coated Metal Arc WeldingNot Recommended
Machinability Rating80
Common Fabrication Processes
  • Casting
    
Thermal Properties
Treatment Value* Time**
* Temperature is measured in Fahrenheit. ** Time is measured in minutes.
Stress Relief500
Solution Treatment0
Typical uses
Product Category Product Reason Category Reason
IndustrialBacks for Lined BearingsCorrosion ResistanceCorrosion Resistance
Backs for Lined BearingsFriction & Wear PropertiesWear Resistance
Backs for Lined BearingsMachining PropertiesMachinability, Good
Bearings for corrosion, lubrication or pressureCorrosion ResistanceCorrosion Resistance
Bearings for corrosion, lubrication or pressureCorrosion ResistanceCorrosion Resistance to Brackish Water
Bearings for corrosion, lubrication or pressureCorrosion ResistanceCorrosion Resistance to Many Industrial Chemicals
Bearings for corrosion, lubrication or pressureCorrosion ResistanceCorrosion Resistance to Numerous Environments
Bearings for corrosion, lubrication or pressureFriction & Wear PropertiesAnti-Seizing Properties
Bearings for corrosion, lubrication or pressureFriction & Wear PropertiesLow Coefficient of Friction
Bearings for corrosion, lubrication or pressureFriction & Wear PropertiesWear Resistance
Bearings for corrosion, lubrication or pressureMachining PropertiesExcellent Machinability
Bushings for corrosion, lubrication or pressureCorrosion ResistanceCorrosion Resistance
Bushings for corrosion, lubrication or pressureCorrosion ResistanceCorrosion Resistance to Brackish Water
Bushings for corrosion, lubrication or pressureCorrosion ResistanceCorrosion Resistance to Many Industrial Chemicals
Bushings for corrosion, lubrication or pressureCorrosion ResistanceCorrosion Resistance to Numerous Environments
Bushings for corrosion, lubrication or pressureFriction & Wear PropertiesAnti-Seizing Properties
Bushings for corrosion, lubrication or pressureFriction & Wear PropertiesLow Coefficient of Friction
Bushings for corrosion, lubrication or pressureFriction & Wear PropertiesWear Resistance
Bushings for corrosion, lubrication or pressureMachining PropertiesExcellent Machinability
Cam Bushings for Diesel EnginesCorrosion ResistanceCorrosion Resistance
Cam Bushings for Diesel EnginesFriction & Wear PropertiesWear Resistance
Cam Bushings for Diesel EnginesMachining PropertiesMachinability, Good
Crankshaft Main BearingsCorrosion ResistanceCorrosion Resistance
Crankshaft Main BearingsFriction & Wear PropertiesAnti-Seizing Properties
Crankshaft Main BearingsFriction & Wear PropertiesLow Coefficient of Friction
Crankshaft Main BearingsMachining PropertiesMachinability, Good
Deep Well Pump Bowl BushingsCorrosion ResistanceCorrosion Resistance
Deep Well Pump Bowl BushingsCorrosion ResistanceCorrosion Resistance to Many Industrial Chemicals
Deep Well Pump Bowl BushingsCorrosion ResistanceCorrosion Resistance to Numerous Environments
Deep Well Pump Bowl BushingsFriction & Wear PropertiesWear Resistance
Deep Well Pump Bowl BushingsMachining PropertiesMachinability, Good
Deep Well Pump Line Shaft BearingsCorrosion ResistanceCorrosion Resistance
Deep Well Pump Line Shaft BearingsCorrosion ResistanceCorrosion Resistance to Many Industrial Chemicals
Deep Well Pump Line Shaft BearingsCorrosion ResistanceCorrosion Resistance to Numerous Environments
Deep Well Pump Line Shaft BearingsFriction & Wear PropertiesWear Resistance
Deep Well Pump Line Shaft BearingsMachining PropertiesMachinability, Good
Electric Motor BearingsCorrosion ResistanceCorrosion Resistance
Electric Motor BearingsFriction & Wear PropertiesAnti-Seizing Properties
Electric Motor BearingsFriction & Wear PropertiesLow Coefficient of Friction
Electric Motor BearingsFriction & Wear PropertiesWear Resistance
Electric Motor BearingsMachining PropertiesMachinability, Good
Flow Monitor ValvesCorrosion ResistanceCorrosion Resistance
Flow Monitor ValvesCorrosion ResistanceCorrosion Resistance to Brackish Water
Flow Monitor ValvesCorrosion ResistanceCorrosion Resistance to Many Industrial Chemicals
Flow Monitor ValvesCorrosion ResistanceCorrosion Resistance to Numerous Environments
Flow Monitor ValvesFriction & Wear PropertiesWear Resistance
Flow Monitor ValvesMachining PropertiesExcellent Machinability
Guide Bushings for Piston RodsCorrosion ResistanceCorrosion Resistance
Guide Bushings for Piston RodsFriction & Wear PropertiesAnti-Seizing Properties
Guide Bushings for Piston RodsFriction & Wear PropertiesLow Coefficient of Friction
Guide Bushings for Piston RodsFriction & Wear PropertiesWear Resistance
Guide Bushings for Piston RodsMachining PropertiesMachinability, Good
Guide Bushings for ValvesCorrosion ResistanceCorrosion Resistance
Guide Bushings for ValvesFriction & Wear PropertiesAnti-Seizing Properties
Guide Bushings for ValvesFriction & Wear PropertiesLow Coefficient of Friction
Guide Bushings for ValvesFriction & Wear PropertiesWear Resistance
Guide Bushings for ValvesMachining PropertiesMachinability, Good
Hydraulic Gland SealsCorrosion ResistanceCorrosion Resistance
Hydraulic Gland SealsFriction & Wear PropertiesAnti-Seizing Properties
Hydraulic Gland SealsFriction & Wear PropertiesLow Coefficient of Friction
Hydraulic Gland SealsFriction & Wear PropertiesWear Resistance
Hydraulic Gland SealsMachining PropertiesMachinability, Good
Locomotive Bearing PartsCorrosion ResistanceCorrosion Resistance
Locomotive Bearing PartsFriction & Wear PropertiesWear Resistance
Locomotive Bearing PartsMachining PropertiesMachinability, Good
Locomotive Bearing PartsMechanical PropertiesResistance to Pounding
Main Bearings for PressesCorrosion ResistanceCorrosion Resistance
Main Bearings for PressesFriction & Wear PropertiesAnti-Seizing Properties
Main Bearings for PressesFriction & Wear PropertiesLow Coefficient of Friction
Main Bearings for PressesFriction & Wear PropertiesWear Resistance
Main Bearings for PressesMachining PropertiesMachinability, Good
Oil Field EquipmentCorrosion ResistanceCorrosion Resistance
Oil Field EquipmentFriction & Wear PropertiesAnti-Seizing Properties
Oil Field EquipmentFriction & Wear PropertiesTolerance for Dirt and Grit
Oil Field EquipmentFriction & Wear PropertiesWear Resistance
Oil Field EquipmentMachining PropertiesMachinability, Good
Piston Pin BearingsCorrosion ResistanceCorrosion Resistance
Piston Pin BearingsFriction & Wear PropertiesAnti-Seizing Properties
Piston Pin BearingsFriction & Wear PropertiesLow Coefficient of Friction
Piston Pin BearingsFriction & Wear PropertiesWear Resistance
Piston Pin BearingsMachining PropertiesMachinability, Good
Pump SleevesCorrosion ResistanceCorrosion Resistance
Pump SleevesCorrosion ResistanceCorrosion Resistance to Numerous Environments
Pump SleevesFriction & Wear PropertiesWear Resistance
Rod BushingsCorrosion ResistanceCorrosion Resistance
Rod BushingsFriction & Wear PropertiesAnti-Seizing Properties
Rod BushingsFriction & Wear PropertiesLow Coefficient of Friction
Rod BushingsFriction & Wear PropertiesWear Resistance
Rod BushingsMachining PropertiesMachinability, Good
Rolling Mill BearingsCorrosion ResistanceCorrosion Resistance
Rolling Mill BearingsFriction & Wear PropertiesAnti-Seizing Properties
Rolling Mill BearingsFriction & Wear PropertiesLow Coefficient of Friction
Rolling Mill BearingsFriction & Wear PropertiesWear Resistance
Rolling Mill BearingsMachining PropertiesMachinability, Good
SealsCorrosion ResistanceCorrosion Resistance
SealsFriction & Wear PropertiesAnti-Seizing Properties
SealsFriction & Wear PropertiesLow Coefficient of Friction
SealsFriction & Wear PropertiesWear Resistance
SealsMachining PropertiesMachinability, Good
Sleeve Bushings (for cranes, etc.)Corrosion ResistanceCorrosion Resistance
Sleeve Bushings (for cranes, etc.)Friction & Wear PropertiesAnti-Seizing Properties
Sleeve Bushings (for cranes, etc.)Friction & Wear PropertiesLow Coefficient of Friction
Sleeve Bushings (for cranes, etc.)Friction & Wear PropertiesWear Resistance
Sleeve Bushings (for cranes, etc.)Machining PropertiesMachinability, Good
Spacer Bushings (for Pumps, etc.)Corrosion ResistanceCorrosion Resistance
Spacer Bushings (for Pumps, etc.)Friction & Wear PropertiesAnti-Seizing Properties
Spacer Bushings (for Pumps, etc.)Friction & Wear PropertiesLow Coefficient of Friction
Spacer Bushings (for Pumps, etc.)Friction & Wear PropertiesWear Resistance
Spacer Bushings (for Pumps, etc.)Machining PropertiesMachinability, Good
Steel Mill BushingsCorrosion ResistanceCorrosion Resistance
Steel Mill BushingsFriction & Wear PropertiesAnti-Seizing Properties
Steel Mill BushingsFriction & Wear PropertiesTolerance for Dirt and Grit
Steel Mill BushingsFriction & Wear PropertiesWear Resistance
Steel Mill BushingsMachining PropertiesMachinability, Good
Wrist Pin BushingsCorrosion ResistanceCorrosion Resistance
Wrist Pin BushingsFriction & Wear PropertiesAnti-Seizing Properties
Wrist Pin BushingsFriction & Wear PropertiesLow Coefficient of Friction
Wrist Pin BushingsFriction & Wear PropertiesWear Resistance
Wrist Pin BushingsMachining PropertiesMachinability, Good
Applicable Specifications
Form System Standard Description
As Centrifugal CastASTMB271/B271MCOPPER BASE ALLOY CENTRIFUGAL CASTINGS
As Continuous CastASTMB505/B505MCOPPER BASE ALLOY CONTINUOUS CASTINGS
As Sand CastASTMB66BRONZE CASTINGS IN THE ROUGH FOR LOCOMOTIVE WEARING PARTS
MILITARYMIL-C-22229COPPER BASE ALLOY CASTINGS (FOR PRESSURE TIGHT APPLICATIONS)
IngotASTMB30COPPER BASE ALLOYS IN INGOT FORM
Corrosion Properties