C93720
| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P(2) | Ni(3) | Sb | |
|
(1) Cu + Sum of Named Elements 99.0% min. (2) For continuous castings P shall be 1.5% max. (3) Ni value includes Co. |
||||||||
| Min (%) | 83.0 | 7.0 | 3.5 | |||||
| Max (%) | 9.0 | 4.5 | 4.0 | 0.7 | 0.10 | 0.50 | 0.50 | |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties