Find suppliers for this alloy
C94000
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P(2) | Ni(3) | Al | S(4) | Sb | Si | |
|
(1) Cu + Sum of Named Elements 98.7% min. (2) For continuous castings P shall be 1.5% max. (3) Ni value includes Co. (4) For continuous castings S shall be 0.25% max. |
|||||||||||
| Min (%) | 69.0 | 14.0 | 12.0 | 0.50 | |||||||
| Max (%) | 72.0 | 16.0 | 14.0 | 0.50 | 0.25 | 0.05 | 1.0 | 0.005 | 0.08 | 0.50 | 0.005 |
| Form | Temper | Temper Code | Brinell Hardness, 500 kg load |
|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||
| As Continuous Cast | As Continuous Cast | M07 | 80 Min for Standard |
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| As Continuous Cast | Castings | ASTM | B505/B505M | COPPER BASE ALLOY CONTINUOUS CASTINGS | |
| Ingot | ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM |
Corrosion Properties