Find suppliers for this alloy
C94100
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P(2) | Ni(3) | Al | S(4) | Sb | Si | |
|
(1) Cu + Sum of Named Elements 98.7% min. (2) For continuous castings P shall be 1.5% max. (3) Ni value includes Co. (4) For continuous castings S shall be 0.25% max. |
|||||||||||
| Min (%) | 72.0 | 18.0 | 4.5 | ||||||||
| Max (%) | 79.0 | 22.0 | 6.5 | 1.0 | 0.25 | 0.50 | 1.0 | 0.005 | 0.08 | 0.8 | 0.005 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
Elongation (%) |
|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||
| As Continuous Cast | As Continuous Cast | M07 |
25 Min for Standard |
7 Min for Standard |
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Industrial | Thrust Block | Corrosion Resistance | Corrosion Resistance |
| Thrust Block | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Thrust Block | Friction & Wear Properties | Low Coefficient of Friction | |
| Thrust Block | Friction & Wear Properties | Wear Resistance | |
| Thrust Block | Machining Characteristics | Excellent Machinability |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| As Continuous Cast | Castings | ASTM | B505/B505M | COPPER BASE ALLOY CONTINUOUS CASTINGS | |
| Bearings & Busings | ASTM | B67 | CAR AND TENDER JOURNAL BEARINGS, LINED | ||
| Ingot | ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM | ||
Corrosion Properties