C94310
| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P(2) | Ni(3) | Sb | |
|
(1) Cu + Sum of Named Elements 99.0% min. (2) For continuous castings P shall be 1.5% max. (3) Ni value includes Co. |
||||||||
| Min (%) | 27.0 | 1.5 | 0.25 | |||||
| Max (%) | Rem | 34.0 | 3.0 | 0.50 | 0.50 | 0.05 | 1.0 | 0.50 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties