Find suppliers for this alloy
C94900
| Elements | ||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni(2) | Al | Mn | S | Sb | Si | |
|
(1) Cu + Sum of Named Elements 99.4% min. (2) Ni value includes Co. |
||||||||||||
| Min (%) | 79.0 | 4.0 | 4.0 | 4.0 | 4.0 | |||||||
| Max (%) | 81.0 | 6.0 | 6.0 | 6.0 | 0.30 | 0.05 | 6.0 | 0.005 | 0.10 | 0.08 | 0.25 | 0.005 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
Elongation (%) |
|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||
| As Sand Cast | As Sand Cast | M01 |
38 Min for Standard 38 Min for Standard |
15 Min for Standard |
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| As Sand Cast | Castings | ASTM | B763/B763M | COPPER ALLOY SAND CASTINGS FOR VALVE APPLICATIONS | |
| Castings | ASTM | B584 | COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS | ||
| Ingot | ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM |
Corrosion Properties