C95200
| Elements | |||
|---|---|---|---|
| Cu(1) | Fe | Al | |
|
(1) Cu + Sum of Named Elements 99.0% min. |
|||
| Min (%) | 86.0 | 2.5 | 8.5 |
| Max (%) | 4.0 | 9.5 | |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Rockwell B scale | Brinell Hardness, 3000 kg load | Shear Strength (ksi) |
Izod (ft-lbs) |
Charpy V-Notch Impact Strength (ft-lbs) |
Charpy Un-Notched Impact Strength | Compressive Strength .001 in. set/in. (ksi) |
Compressive Strength .1 in. set/in. (ksi) |
Creep Strength (0.1% per 10,000 hours) (ksi) |
Fatigue Strength** (ksi) |
Proportional Limit (ksi) |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106. | ||||||||||||||||
| As Centrifugal Cast | As Centrifugal Cast | M02 |
65 Min for Standard 65 Min for Standard |
25 Min for Standard |
20 Min for Standard 20 Min for Standard |
110 Min for Standard |
||||||||||
| As Continuous Cast | As Continuous Cast | M07 |
68 Min for Standard 68 Min for Standard |
26 Min for Standard |
20 Min for Standard 20 Min for Standard |
|||||||||||
| As Permanent Mold Cast | As Permanent Mold Cast | M05 |
93 Typ |
35 Typ |
38 Typ |
78 Typ |
||||||||||
| As Sand Cast | As Sand Cast | M01 |
65 Min for Standard 65 Min for Standard 80 Typ |
25 Min for Standard 27 Typ |
20 Min for Standard 20 Min for Standard 35 Typ |
110 Min for Standard 125 Typ |
40 Typ |
30 Typ | 30 Typ |
20 Typ | 27 Typ | 70 Typ | 7.9 Typ | 22 Typ | 12 Typ | |
| (1)Field Strength 16000 A/m(200 Oersteds) | |
| Melting Point - Liquidus°F | 1913 |
|---|---|
| Melting Point - Solidus°F | 1907 |
| Densitylb/cu in. at 68°F | 0.276 |
| Specific Gravity | 7.64 |
| Electrical Conductivity% IACS at 68°F | 11 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 29.1 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 9 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
| Modulus of Elasticity in Tensionksi | 15000 |
| Magnetic Permeability | 1.1 (1) |
| Poisson's Ratio | 0.31 |
| Casting Attribute | Level |
|---|---|
| Casting Yield | Low |
| Drossing | High |
| Effect of Section Size | Low |
| Fluidity | Medium |
| Gassing | Medium |
| Patternmakers Shrinkage inches per inch | 4/16 |
| Shrinkage in Solidification | High |
| Shrinkage During Freezing | High |
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Brazing | Good |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Excellent |
| Coated Metal Arc Welding | Good |
| Machinability Rating | 20 |
Common Fabrication Processes
| Treatment | Value* | Time** | ||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. ** Time is measured in minutes. | ||||
| Stress Relief | 600 | |||
| Solution Treatment | 0 | |||
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Electrical Hardware | Conductivity (Thermal) | Thermal Conductivity |
| Electrical Hardware | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Electrical Hardware | Mechanical Properties | High Strength | |
| Fasteners | Nuts | Corrosion Resistance | Corrosion Resistance (Excellent) |
| Nuts | Machining Properties | Machinability, Good | |
| Nuts | Mechanical Properties | High Strength | |
| Industrial | Acid Resistant Pumps | Corrosion Resistance | Corrosion Resistance (Excellent) |
| Acid Resistant Pumps | Corrosion Resistance | Corrosion Resistance to Acids | |
| Acid Resistant Pumps | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Acid Resistant Pumps | Corrosion Resistance | Corrosion Resistance to Saline Solutions | |
| Acid Resistant Pumps | Friction & Wear Properties | Wear Resistance | |
| Acid Resistant Pumps | Machining Properties | Machinability, Good | |
| Acid Resistant Pumps | Mechanical Properties | High Strength | |
| Bearing Liners | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Bearing Liners | Friction & Wear Properties | Wear Resistance | |
| Bearing Liners | Mechanical Properties | High Strength | |
| Bearings | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Bearings | Friction & Wear Properties | Wear Resistance | |
| Bearings | Machining Properties | Machinability, Good | |
| Bearings | Mechanical Properties | High Strength | |
| Bushings | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Bushings | Friction & Wear Properties | Wear Resistance | |
| Bushings | Machining Properties | Machinability, Good | |
| Bushings | Mechanical Properties | High Strength | |
| Gears | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Gears | Friction & Wear Properties | Wear Resistance | |
| Gears | Machining Properties | Machinability, Good | |
| Gears | Mechanical Properties | High Strength | |
| High Strength Clamps | Corrosion Resistance | Corrosion Resistance | |
| High Strength Clamps | Mechanical Properties | High Strength | |
| Hot Mill Guides | Conductivity (Thermal) | Thermal Conductivity | |
| Hot Mill Guides | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Hot Mill Guides | Friction & Wear Properties | Wear Resistance | |
| Hot Mill Guides | Mechanical Properties | High Strength | |
| Hot Mill Guides | Mechanical Properties | Retains Strength at Elevated Temperatures | |
| Hydrant Parts | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Hydrant Parts | Corrosion Resistance | Corrosion Resistance to Brackish Water | |
| Hydrant Parts | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Hydrant Parts | Friction & Wear Properties | Wear Resistance | |
| Hydrant Parts | Machining Properties | Machinability, Good | |
| Hydrant Parts | Mechanical Properties | High Strength | |
| Large Gear Parts | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Large Gear Parts | Friction & Wear Properties | Wear Resistance | |
| Large Gear Parts | Mechanical Properties | High Strength | |
| Mild Alkali Applications | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Mild Alkali Applications | Corrosion Resistance | Corrosion Resistance to Acids | |
| Mild Alkali Applications | Friction & Wear Properties | Wear Resistance | |
| Mild Alkali Applications | Mechanical Properties | High Strength | |
| Pickling Equipment | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Pickling Equipment | Corrosion Resistance | Corrosion Resistance to Acids | |
| Pickling Equipment | Machining Properties | Machinability, Good | |
| Pickling Equipment | Mechanical Properties | High Strength | |
| Pickling Tanks | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Pickling Tanks | Corrosion Resistance | Corrosion Resistance to Acids | |
| Pickling Tanks | Friction & Wear Properties | Wear Resistance | |
| Pickling Tanks | Mechanical Properties | High Strength | |
| Plungers | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Plungers | Friction & Wear Properties | Wear Resistance | |
| Plungers | Machining Properties | Machinability, Good | |
| Plungers | Mechanical Properties | High Strength | |
| Pump Parts | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Pump Parts | Corrosion Resistance | Corrosion Resistance to Acids | |
| Pump Parts | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Pump Parts | Corrosion Resistance | Corrosion Resistance to Saline Solutions | |
| Pump Parts | Friction & Wear Properties | Wear Resistance | |
| Pump Parts | Machining Properties | Machinability, Good | |
| Pump Parts | Mechanical Properties | High Strength | |
| Pump Rods | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Pump Rods | Friction & Wear Properties | Wear Resistance | |
| Pump Rods | Machining Properties | Machinability, Good | |
| Pump Rods | Mechanical Properties | High Strength | |
| Thrust Pads | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Thrust Pads | Friction & Wear Properties | Wear Resistance | |
| Thrust Pads | Mechanical Properties | High Strength | |
| Valve Bodies | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Valve Bodies | Friction & Wear Properties | Wear Resistance | |
| Valve Bodies | Machining Properties | Machinability, Good | |
| Valve Bodies | Mechanical Properties | High Strength | |
| Valve Seats | Corrosion Resistance | Corrosion Resistance | |
| Valve Seats | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Valve Seats | Friction & Wear Properties | Wear Resistance | |
| Valve Seats | Machining Properties | Machinability, Good | |
| Valve Seats | Mechanical Properties | High Strength | |
| Valves | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Valves | Friction & Wear Properties | Wear Resistance | |
| Valves | Machining Properties | Machinability, Good | |
| Valves | Mechanical Properties | High Strength | |
| Wear Plates | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Wear Plates | Friction & Wear Properties | Wear Resistance | |
| Wear Plates | Mechanical Properties | High Strength | |
| Welding Jaws | Conductivity (Thermal) | Thermal Conductivity | |
| Welding Jaws | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Welding Jaws | Mechanical Properties | High Strength | |
| Welding Jaws | Mechanical Properties | Retains Strength at Elevated Temperatures | |
| Worm Wheels | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Worm Wheels | Friction & Wear Properties | Wear Resistance | |
| Worm Wheels | Machining Properties | Machinability, Good | |
| Worm Wheels | Mechanical Properties | High Strength | |
| Worms | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Worms | Friction & Wear Properties | Wear Resistance | |
| Worms | Machining Properties | Machinability, Good | |
| Worms | Mechanical Properties | High Strength | |
| Marine | Covers for Marine Hardware | Appearance | Appearance |
| Covers for Marine Hardware | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Covers for Marine Hardware | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Covers for Marine Hardware | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Covers for Marine Hardware | Mechanical Properties | High Strength | |
| Marine Engines | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Marine Engines | Corrosion Resistance | Corrosion Resistance to Brackish Water | |
| Marine Engines | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Marine Engines | Friction & Wear Properties | Wear Resistance | |
| Marine Engines | Mechanical Properties | Fatigue Properties | |
| Marine Engines | Mechanical Properties | High Strength | |
| Marine Hardware | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Marine Hardware | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Marine Hardware | Corrosion Resistance | Corrosion Resistance to Saline Solutions | |
| Marine Hardware | Mechanical Properties | High Strength | |
| Propellers | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Propellers | Corrosion Resistance | Corrosion Resistance to Brackish Water | |
| Propellers | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Propellers | Friction & Wear Properties | Wear Resistance | |
| Propellers | Mechanical Properties | High Strength | |
| Propellers | Mechanical Properties | Retains Strength at Elevated Temperatures | |
| Ordnance | Gun Mountings | Corrosion Resistance | Corrosion Resistance (Excellent) |
| Gun Mountings | Friction & Wear Properties | Wear Resistance | |
| Gun Mountings | Mechanical Properties | High Strength | |
| Gun Slides | Corrosion Resistance | Corrosion Resistance (Excellent) | |
| Gun Slides | Friction & Wear Properties | Wear Resistance | |
| Gun Slides | Mechanical Properties | High Strength |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| As Centrifugal Cast | Castings | SAE | J461 | WROUGHT AND CAST COPPER ALLOYS | |
| Castings | ASME | SB271 | COPPER BASE ALLOY CENTRIFUGAL CASTINGS | ||
| Castings | SAE | J462 | CAST COPPER ALLOYS | ||
| Castings | ASTM | B271/B271M | COPPER BASE ALLOY CENTRIFUGAL CASTINGS | ||
| As Continuous Cast | Castings | SAE | J461 | WROUGHT AND CAST COPPER ALLOYS | |
| Castings | ASME | SB505 | COPPER BASE ALLOY CONTINUOUS CASTINGS | ||
| Castings | SAE | J462 | CAST COPPER ALLOYS | ||
| Castings | ASTM | B505/B505M | COPPER BASE ALLOY CONTINUOUS CASTINGS | ||
| As Sand Cast | Castings | ASME | SB148 | ALUMINUM BRONZE SAND CASTINGS | |
| Castings | SAE | J462 | CAST COPPER ALLOYS | ||
| Castings | ASTM | B763/B763M | COPPER ALLOY SAND CASTINGS FOR VALVE APPLICATIONS | ||
| Castings | ASTM | B148 | ALUMINUM BRONZE SAND CASTINGS | ||
| Castings | SAE | J461 | WROUGHT AND CAST COPPER ALLOYS | ||
| Flanges | ASME | B16.24 | BRONZE PIPE FLANGES AND FLANGED FITTINGS | ||
| ASME | SB148 | ALUMINUM BRONZE SAND CASTINGS | |||
| ASTM | B148 | ALUMINUM BRONZE SAND CASTINGS | |||
| Ingot | |||||
| ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM | |||
| Valves |
Corrosion Properties