C95430
| Elements | ||||
|---|---|---|---|---|
| Cu | Ni | Al | Mn | |
| Min (%) | 10.5 | |||
| Max (%) | Rem | 0.50 | 12.0 | 0.50 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties