| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu(1) | Sn | Zn | Fe | Ni(2) | Al | Mn | |
|
(1) Cu + Sum of Named Elements 99.8% min. (2) Ni value includes Co. |
|||||||
| Min (%) | 78.0 | 2.0 | 4.5 | 9.7 | |||
| Max (%) | 0.20 | 0.30 | 3.5 | 5.5 | 10.9 | 1.5 | |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| As Centrifugal Cast | Castings | AMS | 4880 | ALUMINUM BRONZE CASTINGS, CENTRIFUGAL AND CONTINUOUS CAST, SOLUTION HEAT TREATED AND TEMPERED | |
| Castings | SAE | J461 | WROUGHT AND CAST COPPER ALLOYS | ||
| Castings | SAE | J462 | CAST COPPER ALLOYS |
Corrosion Properties