Find suppliers for this alloyC95700
Chemical Composition
Element
Cu(1)FeNi(2)AlMnSi
(1) Cu + Sum of Named Elements 99.5% min. (2) Ni value includes Co.
Min (%)71.02.01.57.011.0
Max (%)4.03.08.514.00.10
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
Rockwell C scale
Brinell Hardness, 3000 kg load
Stress Rupture
(ksi)
Izod
(ft-lbs)
Charpy V-Notch Impact Strength
(ft-lbs)
Compressive Strength .1 in. set/in.
(ksi)
Creep Strength (0.1% per 10,000 hours)
(ksi)
Fatigue Strength**
(ksi)
Proportional Limit
(ksi)
As Continuous CastAs Continuous CastM0790   Min for Standard
40   Min for Standard
15   Min for Standard
As Permanent Mold CastAs Permanent Mold CastM051   Typ
M05129   Typ
75   Typ
25   Typ
M0590   Min for Standard
40   Min for Standard
15   Min for Standard
As Sand CastAs Sand CastM0190   Min for Standard
95   Typ
40   Min for Standard
45   Typ
20   Min for Standard
26   Typ
180   Typ
34   Typ
68   Typ
5.7   Typ
25   Typ
30   Typ
150   Typ
9.6   Typ
4.2   Typ
4.5   Typ
33   Typ
22   Typ
* Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106.
Physical Properties
(1) Annealed, Fast Cooled Condition
(2) Slow Cooled Condition, Range 2.2 to 15.0
Melting Point - Liquidus°F1814
Melting Point - Solidus°F1742
Densitylb/cu in. at 68°F0.272
Specific Gravity7.53
Electrical Conductivity% IACS at 68°F3
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F7
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)9.8
Specific Heat CapacityBtu/ lb /°F at 68°F0.105
Modulus of Elasticity in Tensionksi18000
Magnetic Permeability1.03(1)
Magnetic Permeability2.2(2)
Poisson's Ratio0.326
Casting Characteristics
Casting Attribute Level
Casting YieldLow
DrossingHigh
Effect of Section SizeLow
FluidityMedium
GassingMedium
Patternmakers Shrinkageinches per inch3/16
Shrinkage in SolidificationHigh
Fabrication Properties
Technique Suitability
SolderingGood
BrazingGood
Oxyacetylene WeldingNot Recommended
Gas Shielded Arc WeldingExcellent
Coated Metal Arc WeldingGood
Machinability Rating50
Common Fabrication Processes
  • Casting
    
Thermal Properties
Treatment Value* Time**
* Temperature is measured in Fahrenheit. ** Time is measured in minutes.
Stress Relief600
Solution Treatment0
Typical uses
Product Category Product Reason Category Reason
ConsumerSafety ToolsCorrosion ResistanceCorrosion Resistance (Excellent)
Safety ToolsMechanical PropertiesHigh Strength
Safety ToolsNon-MagneticNon-Magnetic
Safety ToolsNon-SparkingNon-Sparking
FastenersNutsCorrosion ResistanceCorrosion Resistance (Excellent)
NutsMechanical PropertiesHigh Strength
Stator ClampsCorrosion ResistanceCorrosion Resistance (Excellent)
Stator ClampsMechanical PropertiesFatigue Strength
Stator ClampsMechanical PropertiesHigh Strength
IndustrialBushingsCorrosion ResistanceCorrosion Resistance (Excellent)
BushingsFriction & Wear PropertiesWear Resistance
BushingsMechanical PropertiesHigh Strength
GearsCorrosion ResistanceCorrosion Resistance (Excellent)
GearsFriction & Wear PropertiesWear Resistance
GearsMechanical PropertiesHigh Strength
Hot Mill GuidesCorrosion ResistanceCorrosion Resistance (Excellent)
Hot Mill GuidesFriction & Wear PropertiesWear Resistance
Hot Mill GuidesMechanical PropertiesHigh Strength
Hot Mill GuidesMechanical PropertiesRetains Strength at Elevated Temperatures
ImpellersCorrosion ResistanceCorrosion Resistance (Excellent)
ImpellersFriction & Wear PropertiesWear Resistance
ImpellersMechanical PropertiesHigh Strength
Pickling EquipmentCorrosion ResistanceCorrosion Resistance (Excellent)
Pickling EquipmentCorrosion ResistanceCorrosion Resistance to Acids
Pickling EquipmentMechanical PropertiesHigh Strength
PropellersCorrosion ResistanceCorrosion Resistance
PropellersCorrosion ResistanceCorrosion Resistance (Excellent)
PropellersFriction & Wear PropertiesWear Resistance
PropellersFriction & Wear PropertiesWear Resistance
PropellersMechanical PropertiesFatigue Strength
PropellersMechanical PropertiesFatigue Strength
PropellersMechanical PropertiesHigh Strength
PropellersMechanical PropertiesHigh Strength
Pump CasingsCorrosion ResistanceCorrosion Resistance (Excellent)
Pump CasingsFriction & Wear PropertiesWear Resistance
Pump CasingsMachining PropertiesMachinability, Good
Pump CasingsMechanical PropertiesHigh Strength
Pump CastingsCorrosion ResistanceCorrosion Resistance (Excellent)
Pump CastingsFriction & Wear PropertiesWear Resistance
Pump CastingsMachining PropertiesMachinability, Good
Pump CastingsMechanical PropertiesHigh Strength
Stator Clamp SegmentsCorrosion ResistanceCorrosion Resistance
Stator Clamp SegmentsFriction & Wear PropertiesWear Resistance
Stator Clamp SegmentsMechanical PropertiesFatigue Strength
Stator Clamp SegmentsMechanical PropertiesHigh Strength
ValvesCorrosion ResistanceCorrosion Resistance (Excellent)
ValvesFriction & Wear PropertiesWear Resistance
ValvesMechanical PropertiesHigh Strength
Wear PlatesCorrosion ResistanceCorrosion Resistance (Excellent)
Wear PlatesFriction & Wear PropertiesWear Resistance
Wear PlatesMechanical PropertiesHigh Strength
Welding RodsCorrosion ResistanceCorrosion Resistance (Excellent)
Welding RodsMechanical PropertiesHigh Strength
Worm WheelsCorrosion ResistanceCorrosion Resistance (Excellent)
Worm WheelsFriction & Wear PropertiesWear Resistance
Worm WheelsMechanical PropertiesHigh Strength
WormsCorrosion ResistanceCorrosion Resistance (Excellent)
WormsFriction & Wear PropertiesWear Resistance
WormsMechanical PropertiesHigh Strength
MarineMarine HardwareAppearanceAppearance
Marine HardwareCorrosion ResistanceCorrosion Resistance (Excellent)
Marine HardwareCorrosion ResistanceCorrosion Resistance to Salt Water
Marine HardwareMechanical PropertiesHigh Strength
Applicable Specifications
Form Sub-Form System Standard Description
As Continuous CastASTMB505/B505MCOPPER BASE ALLOY CONTINUOUS CASTINGS
As Sand CastCastingsASTMB148ALUMINUM BRONZE SAND CASTINGS
Ingot
ASTMB30COPPER BASE ALLOYS IN INGOT FORM
Corrosion Properties

No information available.