C95710
| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni(2) | Al | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Ni value includes Co. |
||||||||||
| Min (%) | 71.0 | 2.0 | 1.5 | 7.0 | 11.0 | |||||
| Max (%) | 0.05 | 1.0 | 0.50 | 4.0 | 0.05 | 3.0 | 8.5 | 14.0 | 0.15 | |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties