C95720
| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | Ni(2) | Al | Cr | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Ni value includes Co. |
||||||||||
| Min (%) | 73.0 | 1.5 | 3.0 | 6.0 | 12.0 | |||||
| Max (%) | 0.03 | 0.10 | 0.10 | 3.5 | 6.0 | 8.0 | 0.09 | 15.0 | 0.10 | |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties