Find suppliers for this alloy
C95810
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Zn | Fe(2) | Ni(3) | Al | Mg | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Fe content shall not exceed Ni content. (3) Fe content shall not exceed Ni content. |
|||||||||
| Min (%) | 79.0 | 3.5 | 4.0 | 8.5 | 0.8 | ||||
| Max (%) | 0.09 | 0.50 | 4.5 | 5.0 | 9.5 | 0.05 | 1.5 | 0.10 | |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties