Find suppliers for this alloy
C95820
Elements | |||||||||
---|---|---|---|---|---|---|---|---|---|
Cu(1) | Pb | Sn | Zn | Fe | Ni(2) | Al | Mn | Si | |
(1) Cu + Sum of Named Elements 99.2% min. (2) Ni value includes Co. |
|||||||||
Min (%) | 77.5 | 4.0 | 4.5 | 9.0 | |||||
Max (%) | 0.02 | 0.20 | 0.20 | 5.0 | 5.8 | 10.0 | 1.5 | 0.10 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Form | Specific Sub-Form | Application | System | Standard | Description |
---|---|---|---|---|---|
As Sand Cast | Castings | ASTM | B148 | ALUMINUM BRONZE SAND CASTINGS |
Corrosion Properties