C95900
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1) | Fe | Ni(2) | Al | Mn | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Ni value includes Co. |
|||||
| Min (%) | 3.0 | 12.0 | |||
| Max (%) | Rem | 5.0 | 0.50 | 13.5 | 1.5 |
| Form | Temper | Temper Code | Brinell Hardness, 3000 kg load |
|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||
| As Centrifugal Cast | As Centrifugal Cast | M02 | 241 Min for Standard |
| As Continuous Cast | As Continuous Cast | M07 | 241 Min for Standard |
| As Sand Cast | As Sand Cast | M01 | 241 Min for Standard |
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
| Treatment | Minimum* | Maximum* | Value* | Time** |
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. ** Time is measured in minutes. | ||||
| Stress Relief | 600 | |||
| Solution Treatment | 0 | |||
| Annealing | 1100 | 1300 | 1 | |
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| As Centrifugal Cast | Castings | ASTM | B271/B271M | COPPER BASE ALLOY CENTRIFUGAL CASTINGS | |
| As Continuous Cast | ASTM | B505/B505M | COPPER BASE ALLOY CONTINUOUS CASTINGS | ||
| As Sand Cast | Castings | ASTM | B148 | ALUMINUM BRONZE SAND CASTINGS | |
| Ingot | ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM |
Corrosion Properties