| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Fe | P | Ni(2) | C | Mn | S | Si | Nb | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Ni value includes Co. |
||||||||||
| Min (%) | 0.50 | 18.0 | 0.25 | 0.50 | ||||||
| Max (%) | Rem | 0.01 | 1.5 | 0.02 | 22.0 | 0.15 | 1.5 | 0.02 | 0.50 | 1.5 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Brinell Hardness, 500 kg load |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| As Sand Cast | As Sand Cast | M01 |
75 Typ |
55 Typ |
10 Typ |
150 Typ |
| Melting Point - Liquidus°F | 2190 |
|---|---|
| Melting Point - Solidus°F | 2100 |
| Densitylb/cu in. at 68°F | 0.323 |
| Specific Gravity | 8.94 |
| Electrical Conductivity% IACS at 68°F | 6 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 21.3 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 9.1 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
| Modulus of Elasticity in Tensionksi | 20000 |
| Casting Attribute | Level |
|---|---|
| Casting Yield | Low |
| Drossing | High |
| Fluidity | Medium |
| Gassing | Medium |
| Shrinkage in Solidification | High |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Excellent |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Fair |
| Coated Metal Arc Welding | Fair |
| Machinability Rating | 15 |
Common Fabrication Processes
| Treatment | Time** | |||
|---|---|---|---|---|
| ** Time is measured in minutes. | ||||
| Solution Treatment | 0 | |||
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Industrial | Tail shaft Sleeve | Corrosion Resistance | Corrosion Resistance |
| Tail shaft Sleeve | Corrosion Resistance | Resists Erosion and Impingement Corrosion | |
| Tail shaft Sleeve | Mechanical Properties | High Strength | |
| Tail shaft Sleeve | Mechanical Properties | Retains Strength at Elevated Temperatures |
Applicable Specifications