Find suppliers for this alloy
C96700
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Fe | Ni(2) | Be | Mn | Si | Ti | Zr | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Ni value includes Co. |
|||||||||
| Min (%) | 0.40 | 29.0 | 1.1 | 0.40 | 0.15 | 0.15 | |||
| Max (%) | Rem | 0.01 | 1.0 | 33.0 | 1.2 | 1.0 | 0.15 | 0.35 | 0.35 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
Elongation (%) |
|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||
| As Sand Cast | Precipitation Hardened | TF00 |
125 Min for Standard |
10 Min for Standard |
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| As Sand Cast | Castings | ASTM | B770 | COPPER-BERYLLIUM SAND CASTINGS | |
| Ingot | ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM |
Corrosion Properties