Find suppliers for this alloy
C96800
Elements | ||||||||||
---|---|---|---|---|---|---|---|---|---|---|
Cu(1,2) | Pb | Sn | Zn | Fe | Ni(3) | Mg | Mn | Si | Nb | |
(1) The following additional maximum impurity limits shall apply: 0.10% Al, 0.001% B, 0.001% Bi, 0.005% P, 0.0025% S, 0.02% Sb, 0.01%Ti. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
||||||||||
Min (%) | 7.5 | 9.5 | 0.005 | 0.05 | 0.10 | |||||
Max (%) | Rem | 0.005 | 8.5 | 1.0 | 0.50 | 10.5 | 0.15 | 0.30 | 0.05 | 0.30 |
Form | Temper | Temper Code | Tensile Strength (ksi) |
Elongation (%) |
---|---|---|---|---|
* Measured at room temperature, 68°F (20°C). | ||||
As Sand Cast | As Sand Cast | M01 |
125 Min for Standard |
3 Min for Standard |
Spinodal Hardened-Low Strength (ATLS) | TX00 |
135 Min for Standard |
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Treatment | Minimum* | Value* | Time** | Medium |
---|---|---|---|---|
* Temperature is measured in Fahrenheit. ** Time is measured in minutes. | ||||
Solution Treatment | 1500 | 2 | Water | |
Precipitation Treatment | 660 | 5 |
Typical Uses
Form | Specific Sub-Form | Application | System | Standard | Description |
---|---|---|---|---|---|
As Sand Cast | Castings | ASTM | B584 | COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS | |
Ingot | ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM |
Corrosion Properties