Find suppliers for this alloy
C96900
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | Ni(2) | Mg | Mn | Nb | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Ni value includes Co. |
|||||||||
| Min (%) | 7.5 | 14.5 | 0.05 | ||||||
| Max (%) | Rem | 0.02 | 8.5 | 0.50 | 0.50 | 15.5 | 0.15 | 0.30 | 0.10 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| As Continuous Cast | ASTM | B505/B505M | COPPER BASE ALLOY CONTINUOUS CASTINGS |
Corrosion Properties