C98600
| Elements | |||||
|---|---|---|---|---|---|
| Cu | Pb | Sn | Fe | Ag | |
| Min (%) | 60.0 | 30.0 | |||
| Max (%) | 70.0 | 40.0 | 0.50 | 0.35 | 1.5 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties