C98800
| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu(1) | Pb(2) | Sn | Zn | Fe | P | Ag(3) | |
|
(1) Cu value includes Ag. (2) Pb and Ag may be adjusted to modify alloy hardness. (3) Pb and Ag may be adjusted to modify alloy hardness. |
|||||||
| Min (%) | 56.5 | 37.5 | |||||
| Max (%) | 62.5 | 42.5 | 0.25 | 0.10 | 0.35 | 0.02 | 5.5 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties