C98820
| Elements | ||||
|---|---|---|---|---|
| Cu | Pb | Sn | Fe | |
| Min (%) | 40.0 | 1.0 | ||
| Max (%) | Rem | 44.0 | 5.0 | 0.35 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties