Find suppliers for this alloy
C99600
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | Ni | Al | C | Co | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.7% min. |
|||||||||||
| Min (%) | 1.0 | 39.0 | |||||||||
| Max (%) | Rem | 0.02 | 0.10 | 0.20 | 0.20 | 0.20 | 2.8 | 0.05 | 0.20 | 45.0 | 0.10 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties