C99650
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1) | Pb | Al | C | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.8% min. |
||||||
| Min (%) | 33.0 | |||||
| Max (%) | Rem | 0.02 | 0.10 | 0.30 | 38.0 | 0.10 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Brinell Hardness, 500 kg load |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| As Sand Cast | As Sand Cast | M01 |
41 Typ |
26 Typ |
22 Typ |
82 Typ |
| Melting Point - Liquidus°F | 1603 |
|---|---|
| Densitylb/cu in. at 68°F | 0.274 |
| Specific Gravity | 7.58 |
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties