Find suppliers for this alloy
C99710
| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni | Al | Mn | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.7% min. |
||||||||
| Min (%) | 60.0 | 19.0 | 4.0 | 11.0 | ||||
| Max (%) | 0.09 | 1.0 | 25.0 | 1.0 | 6.0 | 1.0 | 15.0 | |
Mechanical Properties
| Melting Point - Liquidus°F | 1656 |
|---|---|
| Melting Point - Solidus°F | 1615 |
| Densitylb/cu in. at 68°F | 0.301 |
| Specific Gravity | 8.33 |
| Electrical Conductivity% IACS at 68°F | 10 |
| Casting Attribute | Level |
|---|---|
| Casting Yield | Medium |
| Drossing | Medium |
| Effect of Section Size | Low |
| Fluidity | High |
| Gassing | Low |
| Patternmakers Shrinkage inches per inch | 4/16 |
| Shrinkage in Solidification | Medium |
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Brazing | Good |
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications