C99710
Elements | ||||||||
---|---|---|---|---|---|---|---|---|
Cu(1,2) | Pb | Sn | Zn | Fe | Ni | Al | Mn | |
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.7% min. |
||||||||
Min (%) | 60.0 | 19.0 | 4.0 | 11.0 | ||||
Max (%) | 0.09 | 1.0 | 25.0 | 1.0 | 6.0 | 1.0 | 15.0 |
Mechanical Properties
Melting Point - Liquidus°F | 1656 |
---|---|
Melting Point - Solidus°F | 1615 |
Densitylb/cu in. at 68°F | 0.301 |
Specific Gravity | 8.33 |
Electrical Conductivity% IACS at 68°F | 10 |
Casting Attribute | Level |
---|---|
Casting Yield | Medium |
Drossing | Medium |
Effect of Section Size | Low |
Fluidity | High |
Gassing | Low |
Patternmakers Shrinkage inches per inch | 4/16 |
Shrinkage in Solidification | Medium |
Technique | Suitability |
---|---|
Soldering | Good |
Brazing | Good |