Find suppliers for this alloy
C99740
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni | Al | Bi | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.8% min. |
|||||||||||
| Min (%) | 55.0 | 1.5 | 17.0 | 0.6 | 5.0 | 1.0 | 3.0 | 11.0 | |||
| Max (%) | 60.0 | 0.05 | 2.0 | 23.0 | 1.0 | 0.05 | 6.0 | 1.4 | 4.0 | 14.0 | 0.05 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Brinell Hardness, 3000 kg load |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| As Sand Cast | As Sand Cast | M01 |
55 Typ |
32 Typ |
6 Typ |
140 Typ |
Physical Properties
Casting Characteristics
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Brazing | Good |
| Oxyacetylene Welding | Good |
| Machinability Rating | 75 |
Common Fabrication Processes
| Treatment | Minimum* | |||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. | ||||
| Stress Relief | 700 | |||
Typical Uses
Applicable Specifications
Corrosion Properties