Find suppliers for this alloy
C99760
| Elements | |||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni(2) | Al | C | Mn | S | Sb | Si | |
|
(1) Cu + Sum of Named Elements 99.3% min. (2) Ni value includes Co. |
|||||||||||||
| Min (%) | 61.0 | 0.20 | 8.0 | 8.0 | 10.0 | 0.10 | |||||||
| Max (%) | 67.0 | 0.09 | 1.0 | 14.0 | 0.6 | 0.05 | 12.0 | 0.6 | 0.10 | 16.0 | 0.25 | 1.0 | 0.05 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Brinell Hardness, 500 kg load |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| As Permanent Mold Cast | As Permanent Mold Cast | M05 |
39.6 Min 44.5 Typ |
24.9 Min 26.1 Typ |
9 Min 13 Typ |
82 Typ |
| As Sand Cast | As Sand Cast | M01 |
40.6 Min 44.9 Typ |
18.8 Min 21.7 Typ |
23 Min 35 Typ |
71 Typ |
| Melting Point - Liquidus°F | 1868 |
|---|---|
| Melting Point - Solidus°F | 1647 |
| Densitylb/cu in. at 68°F | 0.298 |
| Specific Gravity | 8.26 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.0934 |
| Modulus of Elasticity in Tensionksi | 15500 |
| Magnetic Permeability | 1 |
| Casting Attribute | Level |
|---|---|
| Casting Yield | High |
| Drossing | Medium |
| Effect of Section Size | High |
| Fluidity | Medium |
| Gassing | Medium |
| Patternmakers Shrinkage inches per inch | 3/16 |
| Shrinkage in Solidification | Medium |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties