C99771
| Elements | |||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni(2) | Al | C | Mn | S | Sb | Si | |
|
(1) Cu + Sum of Named Elements 99.3% min. (2) Ni value includes Co. |
|||||||||||||
| Min (%) | 62.0 | 0.20 | 16.0 | 2.0 | 0.01 | 8.0 | 0.10 | ||||||
| Max (%) | 70.0 | 0.09 | 1.5 | 21.0 | 0.6 | 0.05 | 4.0 | 2.0 | 0.10 | 12.0 | 0.25 | 1.0 | 0.05 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties