C99780
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni | Al | Bi | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.8% min. |
|||||||||||
| Min (%) | 62.0 | 0.50 | 16.0 | 4.0 | 0.30 | 0.50 | 12.0 | ||||
| Max (%) | 66.0 | 0.05 | 2.0 | 20.0 | 0.50 | 0.05 | 6.0 | 1.0 | 2.0 | 15.0 | 0.05 |
| Form | Temper | Temper Code | YS-0.5% Ext (ksi) |
Elongation (%) |
Brinell Hardness, 3000 kg load | Torsion Modulus (ksi) |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| As Sand Cast | As Sand Cast | M01 | 25 Typ |
18 Typ |
112 Typ |
46 Typ |
Physical Properties
Casting Characteristics
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Brazing | Good |
| Oxyacetylene Welding | Good |
| Machinability Rating | 70 |
Common Fabrication Processes
| Treatment | Minimum* | |||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. | ||||
| Stress Relief | 700 | |||
Typical Uses
Applicable Specifications
Corrosion Properties