Alloy UNS# | Designation | Active | View |
---|---|---|---|
C14181 * |
Yes |
C14181 Profile Suppliers of C14181 |
|
C14300 * |
Cadmium Copper, Deoxidized | Yes |
C14300 Profile Suppliers of C14300 |
C14310 * |
Cadmium Copper | No |
C14310 Profile Suppliers of C14310 |
C16200 * |
Cadmium Copper | Yes |
C16200 Profile Suppliers of C16200 |
C16210 * |
High Copper Alloy | No |
C16210 Profile Suppliers of C16210 |
C16400 * |
High Copper Alloy | No |
C16400 Profile Suppliers of C16400 |
C16500 * |
Yes |
C16500 Profile Suppliers of C16500 |
|
C49250 * |
Copper-Zinc-Bismuth (Copper-Zinc-Bismuth) | Yes |
C49250 Profile Suppliers of C49250 |
C49260 * |
GEM Brass | Yes |
C49260 Profile Suppliers of C49260 |
C49300 * |
Lead-Free Bismuth Alloy (Lead-Free) | Yes |
C49300 Profile Suppliers of C49300 |
C49340 * |
GEM Brass | Yes |
C49340 Profile Suppliers of C49340 |
C68300 * |
Copper-Znc Alloy (Silicon Modified Brass) | Yes |
C68300 Profile Suppliers of C68300 |
C89560 * |
Copper-Zinc-Bismuth | Yes |
C89560 Profile Suppliers of C89560 |
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |