Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (17) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (14) You Searched For: brazing:"Fair" butt-weld:"Good" CLEAR this search X SAVE this search << Page 1 >> 18 Alloys Found Alloy UNS#DesignationActiveView C18147 Yes C18147 Profile Suppliers of C18147 C18148 Yes C18148 Profile Suppliers of C18148 C42200 * Yes C42200 Profile Suppliers of C42200 C42210 * Tin Brass Yes C42210 Profile Suppliers of C42210 C42220 * Yes C42220 Profile Suppliers of C42220 C53800 Yes C53800 Profile Suppliers of C53800 C60800 Yes C60800 Profile Suppliers of C60800 C61300 * Yes C61300 Profile Suppliers of C61300 C61400 * Yes C61400 Profile Suppliers of C61400 C61900 * Yes C61900 Profile Suppliers of C61900 C62300 * Aluminum Bronze, 9% Yes C62300 Profile Suppliers of C62300 C62400 * Aluminum Bronze,11% Yes C62400 Profile Suppliers of C62400 C63000 * Aluminum Bronze Yes C63000 Profile Suppliers of C63000 C63200 * Aluminum Bronze Yes C63200 Profile Suppliers of C63200 C68800 * Yes C68800 Profile Suppliers of C68800 C69000 * Copper Zinc No C69000 Profile Suppliers of C69000 C87700 * Silicon Bronze (Silicon Bronze) Yes C87700 Profile Suppliers of C87700 C87710 * Silicon Bronze (Silicon Bronze) Yes C87710 Profile Suppliers of C87710 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>