Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
11 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C18147 |
Yes |
C18147 Profile Suppliers of C18147 |
|
C18670 |
MSP5 | Yes |
C18670 Profile Suppliers of C18670 |
C42200 * |
Yes |
C42200 Profile Suppliers of C42200 |
|
C42210 * |
Tin Brass | Yes |
C42210 Profile Suppliers of C42210 |
C42220 * |
Yes |
C42220 Profile Suppliers of C42220 |
|
C63800 * |
Yes |
C63800 Profile Suppliers of C63800 |
|
C66710 |
Yes |
C66710 Profile Suppliers of C66710 |
|
C66907 |
Yes |
C66907 Profile Suppliers of C66907 |
|
C68800 * |
Yes |
C68800 Profile Suppliers of C68800 |
|
C69000 * |
Copper Zinc | No |
C69000 Profile Suppliers of C69000 |
C69750 |
Yes |
C69750 Profile Suppliers of C69750 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |