Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (18) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (12) You Searched For: brazing:"Good" seam-weld:"Fair" CLEAR this search X SAVE this search << Page 1 >> 19 Alloys Found Alloy UNS#DesignationActiveView C17000 * Copper Beryllium Yes C17000 Profile Suppliers of C17000 C17200 * Copper Beryllium Yes C17200 Profile Suppliers of C17200 C17300 Copper Beryllium Yes C17300 Profile Suppliers of C17300 C17400 * Beryllium Copper No C17400 Profile Suppliers of C17400 C17410 * Copper Beryllium Yes C17410 Profile Suppliers of C17410 C17450 * Copper Beryllium Yes C17450 Profile Suppliers of C17450 C17455 Copper Beryllium Yes C17455 Profile Suppliers of C17455 C17460 * Copper Beryllium Yes C17460 Profile Suppliers of C17460 C17465 Copper Beryllium Yes C17465 Profile Suppliers of C17465 C17500 * Copper Beryllium Yes C17500 Profile Suppliers of C17500 C17510 * Copper Beryllium Yes C17510 Profile Suppliers of C17510 C17530 * Copper Beryllium Yes C17530 Profile Suppliers of C17530 C46750 Yes C46750 Profile Suppliers of C46750 C53400 Phosphor Bronze B-1 Yes C53400 Profile Suppliers of C53400 C68700 * Aluminum Brass, Arsenical Yes C68700 Profile Suppliers of C68700 C70315 STOL 94 Yes C70315 Profile Suppliers of C70315 C70330 Yes C70330 Profile Suppliers of C70330 C70350 * Yes C70350 Profile Suppliers of C70350 C72660 * Yes C72660 Profile Suppliers of C72660 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>