6 Alloys Found

Alloy UNS#DesignationActiveView

C84200

Yes C84200 Profile
Suppliers of C84200

C93500

Yes C93500 Profile
Suppliers of C93500

C93700

Bearing Bronze Yes C93700 Profile
Suppliers of C93700

C93800

Anti-acid Metal Yes C93800 Profile
Suppliers of C93800

C94500

Yes C94500 Profile
Suppliers of C94500

C99500 *

Special Alloys Yes C99500 Profile
Suppliers of C99500
* signifies an alloy registered with the U.S. EPA as Antimicrobial.