Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (7) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (7) You Searched For: butt-weld:"Excellent" element_names:"Zinc" elongation:[24 TO 27] CLEAR this search X SAVE this search << Page 1 >> 7 Alloys Found Alloy UNS#DesignationActiveView C50580 * Yes C50580 Profile Suppliers of C50580 C50780 * Yes C50780 Profile Suppliers of C50780 C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C51100 * Yes C51100 Profile Suppliers of C51100 C51180 * Yes C51180 Profile Suppliers of C51180 C51900 * Yes C51900 Profile Suppliers of C51900 C65100 * Low-Silicon Bronze B Yes C65100 Profile Suppliers of C65100 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>