Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (5) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (5) You Searched For: butt-weld:"Excellent" yield-strength:[70 TO 90] oxyacetylene-welding:"Not Recommended" CLEAR this search X SAVE this search << Page 1 >> 5 Alloys Found Alloy UNS#DesignationActiveView C16500 * Yes C16500 Profile Suppliers of C16500 C19040 * CAC5 (High Copper) Yes C19040 Profile Suppliers of C19040 C19050 * SPKFC-5E (High Copper) Yes C19050 Profile Suppliers of C19050 C19250 * SPKFC-5W (High Copper) Yes C19250 Profile Suppliers of C19250 C61500 * Yes C61500 Profile Suppliers of C61500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>