Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (19) Inactive Alloys (5) U.S. EPA Registered Antimicrobial (0) You Searched For: butt-weld:"Fair" electrical-conductivity:[25.0 TO 30.0] CLEAR this search X SAVE this search << Page 1 >> 24 Alloys Found Alloy UNS#DesignationActiveView C33000 Low Leaded Brass (Tube) Yes C33000 Profile Suppliers of C33000 C33100 Leaded Brass No C33100 Profile Suppliers of C33100 C33200 High Leaded Brass (Tube) Yes C33200 Profile Suppliers of C33200 C33500 Low-Leaded Brass Yes C33500 Profile Suppliers of C33500 C34000 Medium Leaded Brass, 64-1/2% Yes C34000 Profile Suppliers of C34000 C34200 High Leaded Brass, 64-1/2% Yes C34200 Profile Suppliers of C34200 C34500 Yes C34500 Profile Suppliers of C34500 C35000 Medium Leaded Brass, 62% Yes C35000 Profile Suppliers of C35000 C35300 High Leaded Brass, 62% Yes C35300 Profile Suppliers of C35300 C35600 Extra High Leaded Brass Yes C35600 Profile Suppliers of C35600 C36000 Free-Cutting Brass Yes C36000 Profile Suppliers of C36000 C36010 Leaded Brass (Free-Cutting Brass) Yes C36010 Profile Suppliers of C36010 C36200 Leaded Brass No C36200 Profile Suppliers of C36200 C36300 Copper-Zinc-Lead Alloy Yes C36300 Profile Suppliers of C36300 C36500 Leaded Muntz Metal, Uninhibited Yes C36500 Profile Suppliers of C36500 C36600 Leaded Muntz Metal, Arsinical No C36600 Profile Suppliers of C36600 C36700 Leaded Muntz Metal, Antimonial No C36700 Profile Suppliers of C36700 C36800 Leaded Brass No C36800 Profile Suppliers of C36800 C37000 Free-Cutting Muntz Metal Yes C37000 Profile Suppliers of C37000 C37100 Yes C37100 Profile Suppliers of C37100 C37700 Forging Brass Yes C37700 Profile Suppliers of C37700 C38500 Architectural Bronze Yes C38500 Profile Suppliers of C38500 C48200 Naval Brass, Medium Leaded Yes C48200 Profile Suppliers of C48200 C48500 Naval Brass, High Leaded Yes C48500 Profile Suppliers of C48500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>