Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (9) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (4) You Searched For: butt-weld:"Not Recommended" capacity-for-being-hot-formed:"Good" CLEAR this search X SAVE this search << Page 1 >> 9 Alloys Found Alloy UNS#DesignationActiveView C18020 Yes C18020 Profile Suppliers of C18020 C18025 High Copper Alloy Yes C18025 Profile Suppliers of C18025 C18660 * High Copper Alloy Yes C18660 Profile Suppliers of C18660 C48640 Yes C48640 Profile Suppliers of C48640 C48645 Yes C48645 Profile Suppliers of C48645 C64770 * Yes C64770 Profile Suppliers of C64770 C64790 Yes C64790 Profile Suppliers of C64790 C70240 * Yes C70240 Profile Suppliers of C70240 C85550 * Low Silicon Brass Yes C85550 Profile Suppliers of C85550 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>