Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (19) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (15) You Searched For: capacity-for-being-cold-worked:"Excellent" butt-weld:"Good" melting-point-liquidus:[1800 TO 1900] CLEAR this search X SAVE this search << Page 1 >> 19 Alloys Found Alloy UNS#DesignationActiveView C22600 * Jewelry Bronze, 87-1/2% Yes C22600 Profile Suppliers of C22600 C23000 * Red Brass, 85% Yes C23000 Profile Suppliers of C23000 C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C41300 * Tin Brass Yes C41300 Profile Suppliers of C41300 C41500 * Tin Brass Yes C41500 Profile Suppliers of C41500 C42300 Yes C42300 Profile Suppliers of C42300 C42500 * Yes C42500 Profile Suppliers of C42500 C42520 * Yes C42520 Profile Suppliers of C42520 C42600 * Yes C42600 Profile Suppliers of C42600 C43000 * Tin Brass Yes C43000 Profile Suppliers of C43000 C43400 * Yes C43400 Profile Suppliers of C43400 C43500 * Tin Brass Yes C43500 Profile Suppliers of C43500 C49100 Yes C49100 Profile Suppliers of C49100 C66420 * Yes C66420 Profile Suppliers of C66420 C66430 * Yes C66430 Profile Suppliers of C66430 C74500 * Nickel Silver, 65-10 Yes C74500 Profile Suppliers of C74500 C75700 * Nickel Silver, 65-12 Yes C75700 Profile Suppliers of C75700 C76200 Nickel Silver Yes C76200 Profile Suppliers of C76200 C77100 Yes C77100 Profile Suppliers of C77100 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>