Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
14 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C17410 * |
Copper Beryllium | Yes |
C17410 Profile Suppliers of C17410 |
C17460 * |
Copper Beryllium | Yes |
C17460 Profile Suppliers of C17460 |
C17465 |
Copper Beryllium | Yes |
C17465 Profile Suppliers of C17465 |
C17540 |
CW103C | Yes |
C17540 Profile Suppliers of C17540 |
C24000 * |
Low Brass, 80% | Yes |
C24000 Profile Suppliers of C24000 |
C42600 * |
Yes |
C42600 Profile Suppliers of C42600 |
|
C51000 * |
Phosphor Bronze, 5% A | Yes |
C51000 Profile Suppliers of C51000 |
C51980 * |
Yes |
C51980 Profile Suppliers of C51980 |
|
C64751 |
Yes |
C64751 Profile Suppliers of C64751 |
|
C64752 |
Yes |
C64752 Profile Suppliers of C64752 |
|
C70252 * |
Copper Nickel (NKC 388) | Yes |
C70252 Profile Suppliers of C70252 |
C70370 * |
Yes |
C70370 Profile Suppliers of C70370 |
|
C72660 * |
Yes |
C72660 Profile Suppliers of C72660 |
|
C74500 * |
Nickel Silver, 65-10 | Yes |
C74500 Profile Suppliers of C74500 |
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |