Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (4) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (5) You Searched For: capacity-for-being-cold-worked:"Excellent" electrical-conductivity:[35.0 TO 40.0] coated-metal-arc-welding:"Fair" CLEAR this search X SAVE this search << Page 1 >> 5 Alloys Found Alloy UNS#DesignationActiveView C17400 * Beryllium Copper No C17400 Profile Suppliers of C17400 C17530 * Copper Beryllium Yes C17530 Profile Suppliers of C17530 C40950 * Yes C40950 Profile Suppliers of C40950 C50780 * Yes C50780 Profile Suppliers of C50780 C70280 * Yes C70280 Profile Suppliers of C70280 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>