Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (4) Inactive Alloys (2) U.S. EPA Registered Antimicrobial (6) You Searched For: capacity-for-being-cold-worked:"Excellent" element_names:"Phosphorus" rockwell-30t-scale:[75 TO 80] CLEAR this search X SAVE this search << Page 1 >> 6 Alloys Found Alloy UNS#DesignationActiveView C26100 * Brass No C26100 Profile Suppliers of C26100 C42500 * Yes C42500 Profile Suppliers of C42500 C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C51100 * Yes C51100 Profile Suppliers of C51100 C66430 * Yes C66430 Profile Suppliers of C66430 C69000 * Copper Zinc No C69000 Profile Suppliers of C69000 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>