Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
11 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C26000 * |
Cartridge Brass, 70% | Yes |
C26000 Profile Suppliers of C26000 |
C26100 * |
Brass | No |
C26100 Profile Suppliers of C26100 |
C26130 * |
Yes |
C26130 Profile Suppliers of C26130 |
|
C26200 * |
Yes |
C26200 Profile Suppliers of C26200 |
|
C40800 * |
Silicon Brass | No |
C40800 Profile Suppliers of C40800 |
C40810 * |
Yes |
C40810 Profile Suppliers of C40810 |
|
C40850 * |
Yes |
C40850 Profile Suppliers of C40850 |
|
C40860 * |
Yes |
C40860 Profile Suppliers of C40860 |
|
C41500 * |
Tin Brass | Yes |
C41500 Profile Suppliers of C41500 |
C42520 * |
Yes |
C42520 Profile Suppliers of C42520 |
|
C66700 * |
Manganese Brass | Yes |
C66700 Profile Suppliers of C66700 |
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |