Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (12) Inactive Alloys (3) U.S. EPA Registered Antimicrobial (13) You Searched For: capacity-for-being-cold-worked:"Excellent" rockwell-30t-scale:[45 TO 50] gas-shielded-arc-welding:"Fair" CLEAR this search X SAVE this search << Page 1 >> 15 Alloys Found Alloy UNS#DesignationActiveView C11000 * Electrolytic Tough Pitch (ETP) Yes C11000 Profile Suppliers of C11000 C11300 * Tough Pitch with Ag (STP) Yes C11300 Profile Suppliers of C11300 C11400 * Tough Pitch with Ag (STP) Yes C11400 Profile Suppliers of C11400 C11500 * Tough Pitch with Ag (STP) Yes C11500 Profile Suppliers of C11500 C11600 * Tough Pitch with Ag (STP) Yes C11600 Profile Suppliers of C11600 C12500 * Fire-Refined Tough Pitch (FRTP) Yes C12500 Profile Suppliers of C12500 C12700 * Copper Alloy No C12700 Profile Suppliers of C12700 C12800 * Copper Alloy No C12800 Profile Suppliers of C12800 C12900 * Fire-Refined Tough Pitch with Ag (FRSTP) Yes C12900 Profile Suppliers of C12900 C13000 Copper Alloy No C13000 Profile Suppliers of C13000 C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 C66700 * Manganese Brass Yes C66700 Profile Suppliers of C66700 C74500 * Nickel Silver, 65-10 Yes C74500 Profile Suppliers of C74500 C75400 Nickel Silver, 65-15 Yes C75400 Profile Suppliers of C75400 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>