Saved Copper Alloys

Saved Searches

Copper Alloy Advanced Search Help

We'd Love Your Input

Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.

4 Alloys Found

Alloy UNS#DesignationActiveView

C17500 *

Copper Beryllium Yes C17500 Profile
Suppliers of C17500

C17510 *

Copper Beryllium Yes C17510 Profile
Suppliers of C17510

C18900 *

Yes C18900 Profile
Suppliers of C18900

C69150 *

Copper Zinc Alloy (Copper Zinc Alloy) Yes C69150 Profile
Suppliers of C69150
* signifies an alloy registered with the U.S. EPA as Antimicrobial.