Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (18) Inactive Alloys (2) U.S. EPA Registered Antimicrobial (12) You Searched For: capacity-for-being-cold-worked:"Excellent" yield-strength:[10 TO 30] density:[0.3 TO 0.31] CLEAR this search X SAVE this search << Page 1 >> 20 Alloys Found Alloy UNS#DesignationActiveView C26100 * Brass No C26100 Profile Suppliers of C26100 C26130 * Yes C26130 Profile Suppliers of C26130 C26200 * Yes C26200 Profile Suppliers of C26200 C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 C27400 * Yellow Brass, 63% Yes C27400 Profile Suppliers of C27400 C27453 Copper Zinc Alloy Yes C27453 Profile Suppliers of C27453 C28340 Yes C28340 Profile Suppliers of C28340 C33000 Low Leaded Brass (Tube) Yes C33000 Profile Suppliers of C33000 C33100 Leaded Brass No C33100 Profile Suppliers of C33100 C33200 High Leaded Brass (Tube) Yes C33200 Profile Suppliers of C33200 C44300 * Admiralty, Arsenical Yes C44300 Profile Suppliers of C44300 C44400 * Admiralty, Antimonial Yes C44400 Profile Suppliers of C44400 C44500 * Admiralty, Phosphorized Yes C44500 Profile Suppliers of C44500 C66700 * Manganese Brass Yes C66700 Profile Suppliers of C66700 C66710 Yes C66710 Profile Suppliers of C66710 C66907 Yes C66907 Profile Suppliers of C66907 C68700 * Aluminum Brass, Arsenical Yes C68700 Profile Suppliers of C68700 C74400 * Nickel Silver Yes C74400 Profile Suppliers of C74400 C76200 Nickel Silver Yes C76200 Profile Suppliers of C76200 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>