Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (8) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (5) You Searched For: capacity-for-being-cold-worked:"Excellent" yield-strength:[50 TO 70] modulus-of-elasticity-in-tension:[19000 TO 20000] CLEAR this search X SAVE this search << Page 1 >> 8 Alloys Found Alloy UNS#DesignationActiveView C17500 * Copper Beryllium Yes C17500 Profile Suppliers of C17500 C17510 * Copper Beryllium Yes C17510 Profile Suppliers of C17510 C18090 Yes C18090 Profile Suppliers of C18090 C18135 Yes C18135 Profile Suppliers of C18135 C18160 Yes C18160 Profile Suppliers of C18160 C70265 * Yes C70265 Profile Suppliers of C70265 C70280 * Yes C70280 Profile Suppliers of C70280 C72500 * Yes C72500 Profile Suppliers of C72500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>