Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (6) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (1) You Searched For: capacity-for-being-cold-worked:"Excellent" yield-strength:[70 TO 90] electrical-conductivity:[80.0 TO 85.0] CLEAR this search X SAVE this search << Page 1 >> 7 Alloys Found Alloy UNS#DesignationActiveView C18080 Yes C18080 Profile Suppliers of C18080 C18100 Yes C18100 Profile Suppliers of C18100 C18145 Yes C18145 Profile Suppliers of C18145 C18200 Chromium Copper Yes C18200 Profile Suppliers of C18200 C18400 Chromium Copper Yes C18400 Profile Suppliers of C18400 C18500 High Copper No C18500 Profile Suppliers of C18500 C19210 * Yes C19210 Profile Suppliers of C19210 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>